70-7075-Forging-T6-LE2.000-S-T3-7-6-0F1-C2 — 7075 Forging T6
- Material Id
- 7075 Forging T6 LE2.000 S T3 7 6 0F1 C2
- Temp F
- 70
- E Msi (Msi)
- 10
- Ec Msi (Msi)
- 10.4
- Fcy Ksi (ksi)
- 61
- Fcy Ksi Lt (ksi)
- 59
- Fsu Ksi (ksi)
- 44
- Ftu Ksi (ksi)
- 73
- Ftu Ksi Lt (ksi)
- 71
- Ftu Ksi St (ksi)
- 69
- Fty Ksi (ksi)
- 61
- Fty Ksi Lt (ksi)
- 59
- Fty Ksi St (ksi)
- 58
- G Msi (Msi)
- 3.8
- Basis
- S
- Condition
- T6a
- Density Lb IN3 (lb/in^3)
- 0.101
- Elongation Pct (%)
- 9
- Elongation Pct Lt (%)
- 4
- Elongation Pct St (%)
- 3
- Form
- Hand Forging
- Poisson Ratio
- 0.33
- Specification
- AMS 4126, AMS-a-22771, and AMS-Qq-a-367
- Thickness Range
- <=2.000