Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged vs Ti-5Al-2.5Sn Bar Annealed
Property comparison of Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged and Ti-5Al-2.5Sn Bar Annealed, both titanium alloy.
| Property | Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged | Ti-5Al-2.5Sn Bar Annealed | Difference |
|---|---|---|---|
| Yield strength | 1,130 MPa | 758.4 MPa | -33% |
| Tensile strength | 1,340 MPa | 792.9 MPa | -41% |
| Elongation | 7 % | 10 % | +43% |
| Elastic modulus | 115,000 MPa | 106,869 MPa | -7% |
| Density | 4,600 kg/m³ | 4,484 kg/m³ | -3% |
Difference is Ti-5Al-2.5Sn Bar Annealed relative to Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-4Al-4Mo-2Sn-0.5Si
- standard
- BS TA45 / BS TA47
- heat treatment
- Solution Treated and Aged
- grade
- Ti-5Al-2.5Sn
- standard
- MIL-HDBK-5J
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators