Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged vs Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si (TIMETAL 829) Annealed
Property comparison of Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged and Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si (TIMETAL 829) Annealed, both titanium alloy.
| Property | Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged | Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si (TIMETAL 829) Annealed | Difference |
|---|---|---|---|
| Yield strength | 1,130 MPa | 820 MPa | -27% |
| Tensile strength | 1,340 MPa | 930 MPa | -31% |
| Elongation | 7 % | 9 % | +29% |
| Elastic modulus | 115,000 MPa | 120,000 MPa | +4% |
| Density | 4,600 kg/m³ | 4,540 kg/m³ | -1% |
| Thermal conductivity | 7.52 W/m·K | 6.9 W/m·K | -8% |
| Coefficient of thermal expansion | 0.000009 1/K | 0.000009 1/K | +7% |
| Melting point | 975 °C | 1,015 °C | +4% |
Difference is Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si (TIMETAL 829) Annealed relative to Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Solution Treated and Aged. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-4Al-4Mo-2Sn-0.5Si
- standard
- BS TA45 / BS TA47
- heat treatment
- Solution Treated and Aged
- grade
- Ti-5.5Al-3.5Sn-3Zr-1Nb-0.25Mo-0.3Si
- standard
- BS TA59 / IMI 829
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators