Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Annealed vs Ti-5Al-1Sn-1Zr-1V-0.8Mo (TIMETAL 5111) Annealed
Property comparison of Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Annealed and Ti-5Al-1Sn-1Zr-1V-0.8Mo (TIMETAL 5111) Annealed, both titanium alloy.
| Property | Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Annealed | Ti-5Al-1Sn-1Zr-1V-0.8Mo (TIMETAL 5111) Annealed | Difference |
|---|---|---|---|
| Yield strength | 960 MPa | 775 MPa | -19% |
| Tensile strength | 1,100 MPa | 865 MPa | -21% |
| Elongation | 9 % | 14 % | +56% |
| Elastic modulus | 115,000 MPa | 110,500 MPa | -4% |
| Density | 4,600 kg/m³ | 4,430 kg/m³ | -4% |
| Thermal conductivity | 7.52 W/m·K | 7.5 W/m·K | 0% |
| Coefficient of thermal expansion | 0.000009 1/K | 0.000008 1/K | -7% |
| Melting point | 975 °C | 980 °C | +1% |
| Reduction in area | 20 % | 29 % | +45% |
Difference is Ti-5Al-1Sn-1Zr-1V-0.8Mo (TIMETAL 5111) Annealed relative to Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-4Al-4Mo-2Sn-0.5Si
- standard
- BS TA45 / BS TA47
- heat treatment
- Annealed
- grade
- Ti-5Al-1Sn-1Zr-1V-0.8Mo Grade 32
- standard
- ASTM Grade 32
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators