Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Solution Treated and Aged vs Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Annealed

Property comparison of Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Solution Treated and Aged and Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Annealed, both titanium alloy.

Titanium Alloy3 compared properties
PropertyTi-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Solution Treated and AgedTi-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) AnnealedDifference
Elastic modulus103,400 MPa115,000 MPa+11%
Density4,820 kg/m³4,600 kg/m³-5%
Melting point1,649 °C975 °C-41%

Difference is Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Annealed relative to Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Solution Treated and Aged. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Solution Treated and Aged
grade
Ti-3Al-8V-6Cr-4Mo-4Zr
standard
AMS 4957 / ASTM B348 Grade 19
heat treatment
Solution Treated and Aged
Ti-4Al-4Mo-2Sn-0.5Si (TIMETAL 550) Annealed
grade
Ti-4Al-4Mo-2Sn-0.5Si
standard
BS TA45 / BS TA47
heat treatment
Annealed