Ti-2.5Cu (TIMETAL 230) Solution Treated and Aged vs Ti-3.9V-0.85Al-0.25Si-0.25Fe (TIMETAL 407) STA Water Quench
Property comparison of Ti-2.5Cu (TIMETAL 230) Solution Treated and Aged and Ti-3.9V-0.85Al-0.25Si-0.25Fe (TIMETAL 407) STA Water Quench, both titanium alloy.
| Property | Ti-2.5Cu (TIMETAL 230) Solution Treated and Aged | Ti-3.9V-0.85Al-0.25Si-0.25Fe (TIMETAL 407) STA Water Quench | Difference |
|---|---|---|---|
| Yield strength | 600 MPa | 776 MPa | +29% |
| Tensile strength | 760 MPa | 882 MPa | +16% |
| Elongation | 20 % | 23 % | +15% |
| Density | 4,560 kg/m³ | 4,530 kg/m³ | -1% |
| Thermal conductivity | 12.97 W/m·K | 11.3 W/m·K | -13% |
| Melting point | 890 °C | 890 °C | 0% |
Difference is Ti-3.9V-0.85Al-0.25Si-0.25Fe (TIMETAL 407) STA Water Quench relative to Ti-2.5Cu (TIMETAL 230) Solution Treated and Aged. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-2.5Cu
- standard
- BS TA51 / DTD 5013
- heat treatment
- Solution Treated and Aged
- grade
- Ti-3.9V-0.85Al-0.25Si-0.25Fe
- standard
- TIMET Proprietary
- heat treatment
- Solution Treated and Aged (Water Quench)
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.