Ti-12Mo-6Zr-2Fe (Stryker TMZF) Annealed vs Ti-15Mo (ATI 15Mo) Alpha+Beta Annealed
Property comparison of Ti-12Mo-6Zr-2Fe (Stryker TMZF) Annealed and Ti-15Mo (ATI 15Mo) Alpha+Beta Annealed, both titanium alloy.
| Property | Ti-12Mo-6Zr-2Fe (Stryker TMZF) Annealed | Ti-15Mo (ATI 15Mo) Alpha+Beta Annealed | Difference |
|---|---|---|---|
| Yield strength | 965 MPa | 800 MPa | -17% |
| Tensile strength | 1,000 MPa | 900 MPa | -10% |
| Elongation | 15 % | 10 % | -33% |
| Density | 4,980 kg/m³ | 4,950 kg/m³ | -1% |
Difference is Ti-15Mo (ATI 15Mo) Alpha+Beta Annealed relative to Ti-12Mo-6Zr-2Fe (Stryker TMZF) Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-12Mo-6Zr-2Fe
- standard
- ASTM F1813
- heat treatment
- Annealed (1400°F)
- grade
- Ti-15Mo
- standard
- ASTM F2066
- heat treatment
- Alpha+Beta Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators