Ti-12Mo-6Zr-2Fe (Stryker TMZF) Annealed vs Ti-15Mo-3Nb-3Al-0.2Si (TIMETAL 21S) Solution Treated and Aged
Property comparison of Ti-12Mo-6Zr-2Fe (Stryker TMZF) Annealed and Ti-15Mo-3Nb-3Al-0.2Si (TIMETAL 21S) Solution Treated and Aged, both titanium alloy.
| Property | Ti-12Mo-6Zr-2Fe (Stryker TMZF) Annealed | Ti-15Mo-3Nb-3Al-0.2Si (TIMETAL 21S) Solution Treated and Aged | Difference |
|---|---|---|---|
| Yield strength | 965 MPa | 1,103 MPa | +14% |
| Tensile strength | 1,000 MPa | 1,172 MPa | +17% |
| Elongation | 15 % | 4 % | -73% |
| Density | 4,980 kg/m³ | 4,930 kg/m³ | -1% |
Difference is Ti-15Mo-3Nb-3Al-0.2Si (TIMETAL 21S) Solution Treated and Aged relative to Ti-12Mo-6Zr-2Fe (Stryker TMZF) Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-12Mo-6Zr-2Fe
- standard
- ASTM F1813
- heat treatment
- Annealed (1400°F)
- grade
- Ti-15Mo-3Nb-3Al-0.2Si
- standard
- AMS 4897
- heat treatment
- Solution Treated and Aged (1000°F/8hrs)
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators