| Property | Steel SAE 8630 | Steel SAE 8650 | Difference |
|---|---|---|---|
| Yield strength | 1,503 MPa | 688 MPa | -54% |
| Tensile strength | 1,641 MPa | 1,024 MPa | -38% |
| Elongation | 9 % | 14 % | +56% |
| Elastic modulus | 207,000 MPa | 207,000 MPa | 0% |
| Shear modulus | 79,000 MPa | 79,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Brinell hardness | 465 HB | 302 HB | -35% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 460 J/kg·K | 465 J/kg·K | +1% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is Steel SAE 8650 relative to Steel SAE 8630. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
Steel SAE 8630
- standard
- ANSI
- heat treatment
- tempered at 400 F
Steel SAE 8650
- standard
- ANSI
- heat treatment
- normalized
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators