Rubber Elastomer7 compared properties
PropertyPolyurethane Elastomer (AU/EU Cast 90A)Silicone Rubber (VMQ peroxide-cured)Difference
Tensile strength39 MPa8 MPa-79%
Elongation580 %400 %-31%
Poisson ratio0.480.5+4%
Density1,270 kg/m³1,160 kg/m³-9%
Thermal conductivity0.19 W/m·K0.23 W/m·K+21%
Specific heat1,760 J/kg·K1,400 J/kg·K-20%
Coefficient of thermal expansion0.00015 1/K0.0003 1/K+100%

Difference is Silicone Rubber (VMQ peroxide-cured) relative to Polyurethane Elastomer (AU/EU Cast 90A). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Polyurethane Elastomer (AU/EU Cast 90A)
standard
ASTM
Silicone Rubber (VMQ peroxide-cured)
standard
ASTM