Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Rubber Elastomer/Nitrile Rubber (NBR 33% ACN vulcanized) vs Silicone Rubber (VMQ peroxide-cured)

Nitrile Rubber (NBR 33% ACN vulcanized) vs Silicone Rubber (VMQ peroxide-cured)

Property comparison of Nitrile Rubber (NBR 33% ACN vulcanized) and Silicone Rubber (VMQ peroxide-cured), both rubber elastomer.

Rubber Elastomer7 compared properties
PropertyNitrile Rubber (NBR 33% ACN vulcanized)Silicone Rubber (VMQ peroxide-cured)Difference
Tensile strength15 MPa8 MPa-47%
Elongation450 %400 %-11%
Poisson ratio0.50.50%
Density1,000 kg/m³1,160 kg/m³+16%
Thermal conductivity0.24 W/m·K0.23 W/m·K-4%
Specific heat1,800 J/kg·K1,400 J/kg·K-22%
Coefficient of thermal expansion0.00019 1/K0.0003 1/K+58%

Difference is Silicone Rubber (VMQ peroxide-cured) relative to Nitrile Rubber (NBR 33% ACN vulcanized). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Nitrile Rubber (NBR 33% ACN vulcanized)
standard
ASTM
Silicone Rubber (VMQ peroxide-cured)
standard
ASTM

What else is in Engineering Database

Related comparisons

View each material