NiTiFe (Shape Memory, Ms < -100°C) vs Ti CP Grade 1 (CP-1) Bar Annealed
Property comparison of NiTiFe (Shape Memory, Ms < -100°C) and Ti CP Grade 1 (CP-1) Bar Annealed, both titanium alloy.
| Property | NiTiFe (Shape Memory, Ms < -100°C) | Ti CP Grade 1 (CP-1) Bar Annealed | Difference |
|---|---|---|---|
| Yield strength | 345 MPa | 482.6 MPa | +40% |
| Tensile strength | 1,070 MPa | 551.6 MPa | -48% |
| Elongation | 15 % | 15 % | 0% |
| Density | 6,450 kg/m³ | 4,512 kg/m³ | -30% |
Difference is Ti CP Grade 1 (CP-1) Bar Annealed relative to NiTiFe (Shape Memory, Ms < -100°C). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ni-50-56Ti-2-5Fe
- standard
- ATI Proprietary
- heat treatment
- Solution Annealed
- grade
- Ti CP Grade 1
- standard
- MIL-HDBK-5J
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators