Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Titanium Alloy/NiTiFe (Shape Memory, Ms < -100°C) vs Ti 13V 11CR 3AL

NiTiFe (Shape Memory, Ms < -100°C) vs Ti 13V 11CR 3AL

Property comparison of NiTiFe (Shape Memory, Ms < -100°C) and Ti 13V 11CR 3AL, both titanium alloy.

Titanium Alloy3 compared properties
PropertyNiTiFe (Shape Memory, Ms < -100°C)Ti 13V 11CR 3ALDifference
Yield strength345 MPa827.4 MPa+140%
Tensile strength1,070 MPa861.8 MPa-19%
Elongation15 %10 %-33%

Difference is Ti 13V 11CR 3AL relative to NiTiFe (Shape Memory, Ms < -100°C). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NiTiFe (Shape Memory, Ms < -100°C)
grade
Ni-50-56Ti-2-5Fe
standard
ATI Proprietary
heat treatment
Solution Annealed
Ti 13V 11CR 3AL
grade
Ti-13V-11Cr-3Al
standard
MIL-HDBK-5J
heat treatment
Annealed

What else is in Engineering Database

Related comparisons

View each material