Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Titanium Alloy/NiTi SEA 2 (Superelastic, Af 0°C to 30°C) vs CP Ti Grade 11 (Ti-0.15Pd) Annealed

NiTi SEA 2 (Superelastic, Af 0°C to 30°C) vs CP Ti Grade 11 (Ti-0.15Pd) Annealed

Property comparison of NiTi SEA 2 (Superelastic, Af 0°C to 30°C) and CP Ti Grade 11 (Ti-0.15Pd) Annealed, both titanium alloy.

Titanium Alloy3 compared properties
PropertyNiTi SEA 2 (Superelastic, Af 0°C to 30°C)CP Ti Grade 11 (Ti-0.15Pd) AnnealedDifference
Tensile strength1,070 MPa240 MPa-78%
Elongation10 %24 %+140%
Density6,450 kg/m³4,510 kg/m³-30%

Difference is CP Ti Grade 11 (Ti-0.15Pd) Annealed relative to NiTi SEA 2 (Superelastic, Af 0°C to 30°C). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NiTi SEA 2 (Superelastic, Af 0°C to 30°C)
grade
Ni-55.7Ti (SEA 2)
standard
ASTM F2063
heat treatment
Solution Annealed
CP Ti Grade 11 (Ti-0.15Pd) Annealed
grade
CP Ti Grade 11
standard
ASTM B265 Grade 11
heat treatment
Annealed