NiTi SEA 2 (Superelastic, Af 0°C to 30°C)
Titanium Alloy from the Metal Alloy Properties reference table.
| category | cte per K | density kg m3 | elongation percent | grade | heat treatment | material id | melting point C | name | property basis | standard | tensile strength MPa | thermal conductivity W mK |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| titanium_alloy | 0.000011 | 6,450 | 10 | Ni-55.7Ti (SEA 2) | Solution Annealed | NiTi_SEA2 | 1,310 | NiTi SEA 2 (Superelastic, Af 0°C to 30°C) | Minimum | ASTM F2063 | 1,070 | 18 |
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculatorsRelated titanium alloy materials
NiTiFe (Shape Memory, Ms < -100°C)NiTiNb (Shape Memory, As > 30°C, cryogenic Ms)NiTi SEA 1 (Superelastic, Af -30°C to 0°C)NiTi SMA 1 (Shape Memory, Af 30°C to 75°C)NiTi SMA 2 (Shape Memory, Af 75°C to 120°C)Ti 10V 2FE 3ALTi-11Sn-5Zr-2.25Al-1Mo-0.2Si (TIMETAL 679) AnnealedTi-12Mo-6Zr-2Fe (Stryker TMZF) AnnealedTi-12Mo-6Zr-2Fe (ATI TiOstalloy) AnnealedTi-12Mo-6Zr-2Fe (ATI TiOsteum) AnnealedTi 13V 11CR 3ALTi-15Mo-3Nb-3Al-0.2Si (TIMETAL 21S) Solution Treated and Aged