Nickel 200 vs Nickel 201
Property comparison of Nickel 200 and Nickel 201, both nickel alloy.
| Property | Nickel 200 | Nickel 201 | Difference |
|---|---|---|---|
| Yield strength | 105 MPa | 103 MPa | -2% |
| Tensile strength | 415 MPa | 403 MPa | -3% |
| Elongation | 50 % | 50 % | 0% |
| Elastic modulus | 205,000 MPa | 205,000 MPa | 0% |
| Poisson ratio | 0.29 | 0.29 | 0% |
| Density | 8,890 kg/m³ | 8,890 kg/m³ | 0% |
| Thermal conductivity | 66.5 W/m·K | 66.5 W/m·K | 0% |
| Specific heat | 456 J/kg·K | 456 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000013 1/K | 0.000013 1/K | -2% |
| Melting point | 1,441 °C | 1,441 °C | 0% |
Difference is Nickel 201 relative to Nickel 200. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
Nickel 200
- grade
- 200
- standard
- Special Metals Technical Bulletin SMC-084
- heat treatment
- Annealed
Nickel 201
- grade
- 201
- standard
- Special Metals Technical Bulletin SMC-084
- heat treatment
- Annealed
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators