| Property | MAR-M 247 (Ni-8.3Cr-10Co-10W-5.5Al-3Ta-1Ti-0.7Mo) cast heat treated | Nickel 200 | Difference |
|---|---|---|---|
| Yield strength | 930 MPa | 105 MPa | -89% |
| Tensile strength | 1,035 MPa | 415 MPa | -60% |
| Elongation | 5 % | 50 % | +900% |
| Density | 7,800 kg/m³ | 8,890 kg/m³ | +14% |
| Thermal conductivity | 11.3 W/m·K | 66.5 W/m·K | +488% |
| Coefficient of thermal expansion | 0.000013 1/K | 0.000013 1/K | +6% |
| Melting point | 1,366 °C | 1,441 °C | +5% |
Difference is Nickel 200 relative to MAR-M 247 (Ni-8.3Cr-10Co-10W-5.5Al-3Ta-1Ti-0.7Mo) cast heat treated. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- N/A
- standard
- AZoM Super Alloy MAR-M 247 (ArticleID 7808); TMS Superalloys 1984 Kaufman et al. MAR-M-247 turbine blisk
- heat treatment
- investment cast + standard heat treat
- grade
- 200
- standard
- Special Metals Technical Bulletin SMC-084
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators