Nickel Alloy10 compared properties
PropertyInconel 617 (Ni-22Cr-12Co-9Mo) annealedInconel 625Difference
Yield strength330 MPa448 MPa+36%
Tensile strength740 MPa862 MPa+16%
Elongation55 %50 %-9%
Elastic modulus211,000 MPa207,500 MPa-2%
Density8,360 kg/m³8,440 kg/m³+1%
Brinell hardness170 HB200 HB+18%
Thermal conductivity13.4 W/m·K10.8 W/m·K-19%
Specific heat419 J/kg·K427 J/kg·K+2%
Coefficient of thermal expansion0.000013 1/K0.000013 1/K0%
Melting point1,380 °C1,350 °C-2%

Difference is Inconel 625 relative to Inconel 617 (Ni-22Cr-12Co-9Mo) annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Inconel 617 (Ni-22Cr-12Co-9Mo) annealed
grade
N06617
standard
Special Metals Corp. tech bulletin INCONEL alloy 617 (SMC-029)
heat treatment
solution-annealed
Inconel 625
grade
N06625
standard
Special Metals Corp. tech bulletin INCONEL alloy 625 (SMC-063)
heat treatment
annealed

About Inconel nickel-chromium superalloys

Inconel is a family of nickel-chromium-iron superalloys. They keep strength at temperatures where steels and most stainless grades have failed and resist oxidation and hot corrosion. Inconel 718 is the most widely used grade for aerospace turbine disks and high-temperature fasteners; Inconel 625 is the choice when chloride and reducing-acid corrosion both matter.

What else is in Engineering Database

Related comparisons

View each material