Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Nickel Alloy/Hastelloy C-276 vs Hastelloy X

Hastelloy C-276 vs Hastelloy X

Property comparison of Hastelloy C-276 and Hastelloy X, both nickel alloy.

Nickel Alloy9 compared properties
PropertyHastelloy C-276Hastelloy XDifference
Yield strength360 MPa380 MPa+6%
Tensile strength790 MPa760 MPa-4%
Elongation58 %44 %-24%
Elastic modulus205,000 MPa196,000 MPa-4%
Poisson ratio0.310.32+3%
Density8,890 kg/m³8,220 kg/m³-8%
Thermal conductivity10.2 W/m·K9.7 W/m·K-5%
Coefficient of thermal expansion0.000013 1/K0.000014 1/K+9%
Melting point1,347 °C1,308 °C-3%

Difference is Hastelloy X relative to Hastelloy C-276. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Hastelloy C-276
grade
C-276
standard
Haynes International Datasheet H-2002
heat treatment
Annealed
Hastelloy X
grade
X
standard
Haynes International Datasheet H-3009C
heat treatment
Annealed

About Hastelloy nickel-molybdenum superalloys

Hastelloy is a family of nickel-molybdenum-chromium alloys built for severe corrosion service. C-276 is the workhorse for chemical process equipment and handles wet chlorine, hypochlorite, and ferric chloride. B-series grades focus on hydrochloric acid resistance.

What else is in Engineering Database

Related comparisons

View each material