PropertyEN 16MnCr5EN 17Cr3Difference
Yield strength680 MPa340 MPa-50%
Tensile strength900 MPa580 MPa-36%
Elongation10 %14 %+40%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity66.9 W/m·K51.9 W/m·K-22%
Specific heat456 J/kg·K456 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN 17Cr3 relative to EN 16MnCr5. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN 16MnCr5
standard
ISO
heat treatment
case-hardened
EN 17Cr3
standard
ISO
heat treatment

What else is in Engineering Database

Related comparisons

View each material