Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
DIN Ck50 vs DIN Ck60
Property comparison of DIN Ck50 and DIN Ck60, both carbon steel.
| Property | DIN Ck50 | DIN Ck60 | Difference |
|---|---|---|---|
| Yield strength | 460 MPa | 520 MPa | +13% |
| Tensile strength | 700 MPa | 800 MPa | +14% |
| Elongation | 15 % | 13 % | -13% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 54 W/m·K | 51.9 W/m·K | -4% |
| Specific heat | 465 J/kg·K | 467 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is DIN Ck60 relative to DIN Ck50. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
DIN Ck50
- standard
- DIN
- heat treatment
- face hardened
DIN Ck60
- standard
- DIN
- heat treatment
- heat treated
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators