DIN Ck40 vs DIN Ck50

Property comparison of DIN Ck40 and DIN Ck50, both carbon steel.

Carbon Steel11 compared properties
PropertyDIN Ck40DIN Ck50Difference
Yield strength400 MPa460 MPa+15%
Tensile strength630 MPa700 MPa+11%
Elongation18 %15 %-17%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity57.8 W/m·K54 W/m·K-7%
Specific heat462 J/kg·K465 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN Ck50 relative to DIN Ck40. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN Ck40
standard
DIN
heat treatment
heat treated
DIN Ck50
standard
DIN
heat treatment
face hardened