DIN Ck30 vs DIN Ck40

Property comparison of DIN Ck30 and DIN Ck40, both carbon steel.

Carbon Steel11 compared properties
PropertyDIN Ck30DIN Ck40Difference
Yield strength350 MPa400 MPa+14%
Tensile strength550 MPa630 MPa+15%
Elongation20 %18 %-10%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity61.6 W/m·K57.8 W/m·K-6%
Specific heat460 J/kg·K462 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN Ck40 relative to DIN Ck30. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN Ck30
standard
DIN
heat treatment
DIN Ck40
standard
DIN
heat treatment
heat treated

What else is in Engineering Database

Related comparisons

View each material