Property comparison of DIN Ck30 and DIN Ck45, both carbon steel.

Carbon Steel11 compared properties
PropertyDIN Ck30DIN Ck45Difference
Yield strength350 MPa320 MPa-9%
Tensile strength550 MPa535 MPa-3%
Elongation20 %16 %-20%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity61.6 W/m·K55.9 W/m·K-9%
Specific heat460 J/kg·K464 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN Ck45 relative to DIN Ck30. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN Ck30
standard
DIN
heat treatment
DIN Ck45
standard
DIN
heat treatment
normalized