Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/DIN Ck25 vs DIN Ck35

DIN Ck25 vs DIN Ck35

Property comparison of DIN Ck25 and DIN Ck35, both carbon steel.

Carbon Steel11 compared properties
PropertyDIN Ck25DIN Ck35Difference
Yield strength320 MPa370 MPa+16%
Tensile strength500 MPa600 MPa+20%
Elongation21 %19 %-10%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity63.5 W/m·K59.7 W/m·K-6%
Specific heat458 J/kg·K461 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN Ck35 relative to DIN Ck25. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN Ck25
standard
DIN
DIN Ck35
standard
DIN