PropertyDIN Ck10DIN Ck25Difference
Yield strength275 MPa320 MPa+16%
Tensile strength440 MPa500 MPa+14%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity69.2 W/m·K63.5 W/m·K-8%
Specific heat455 J/kg·K458 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN Ck25 relative to DIN Ck10. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN Ck10
standard
DIN
heat treatment
case-hardened
DIN Ck25
standard
DIN
heat treatment

What else is in Engineering Database