Property comparison of DIN Ck15 and DIN Ck22, both carbon steel.

Carbon Steel10 compared properties
PropertyDIN Ck15DIN Ck22Difference
Yield strength295 MPa300 MPa+2%
Tensile strength495 MPa500 MPa+1%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity67.3 W/m·K64.6 W/m·K-4%
Specific heat456 J/kg·K458 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN Ck22 relative to DIN Ck15. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN Ck15
standard
DIN
heat treatment
case-hardened
DIN Ck22
standard
DIN
heat treatment

What else is in Engineering Database

Related comparisons

View each material