DIN Cf35 vs DIN Ck15

Property comparison of DIN Cf35 and DIN Ck15, both carbon steel.

Carbon Steel10 compared properties
PropertyDIN Cf35DIN Ck15Difference
Yield strength360 MPa295 MPa-18%
Tensile strength580 MPa495 MPa-15%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity59.7 W/m·K67.3 W/m·K+13%
Specific heat461 J/kg·K456 J/kg·K-1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN Ck15 relative to DIN Cf35. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN Cf35
standard
DIN
heat treatment
DIN Ck15
standard
DIN
heat treatment
case-hardened

What else is in Engineering Database

Related comparisons

View each material