Home/Compare/Carbon Steel/DIN 10S2O vs DIN 16MnCr5

DIN 10S2O vs DIN 16MnCr5

Property comparison of DIN 10S2O and DIN 16MnCr5, both carbon steel.

Carbon Steel11 compared properties
PropertyDIN 10S2ODIN 16MnCr5Difference
Yield strength355 MPa680 MPa+92%
Tensile strength460 MPa900 MPa+96%
Elongation9 %10 %+11%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity69.2 W/m·K66.9 W/m·K-3%
Specific heat455 J/kg·K456 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN 16MnCr5 relative to DIN 10S2O. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN 10S2O
standard
DIN
heat treatment
DIN 16MnCr5
standard
DIN
heat treatment
case-hardened