PropertyDIN 10CrMo9-10DIN 16MnCr5Difference
Yield strength300 MPa680 MPa+127%
Tensile strength480 MPa900 MPa+88%
Elongation18 %10 %-44%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity69.2 W/m·K66.9 W/m·K-3%
Specific heat455 J/kg·K456 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN 16MnCr5 relative to DIN 10CrMo9-10. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN 10CrMo9-10
standard
DIN
heat treatment
DIN 16MnCr5
standard
DIN
heat treatment
case-hardened