Custom 450 vs SAE 405 Stainless Steel (Cold drawn bar)

Property comparison of Custom 450 and SAE 405 Stainless Steel (Cold drawn bar), both stainless steel.

Stainless Steel6 compared properties
PropertyCustom 450SAE 405 Stainless Steel (Cold drawn bar)Difference
Yield strength930.8 MPa483 MPa-48%
Tensile strength999.7 MPa586 MPa-41%
Elongation12 %20 %+67%
Elastic modulus193,053 MPa193,000 MPa0%
Density7,750 kg/m³7,850 kg/m³+1%
Reduction in area45 %60 %+33%

Difference is SAE 405 Stainless Steel (Cold drawn bar) relative to Custom 450. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Custom 450
grade
Custom 450
standard
MIL-HDBK-5J
heat treatment
H1050
SAE 405 Stainless Steel (Cold drawn bar)
grade
405
standard
SAE
heat treatment
Cold drawn bar

About 400-series stainless steels

Martensitic and ferritic stainless steels carry less nickel than the 300-series and remain magnetic. 410 and 420 are hardenable by quench and temper and are used for cutlery, shafts, and valve parts. 430 stays soft and is used for cosmetic trim and mild corrosion service. Compared to 300-series grades they trade general corrosion resistance for hardenability.