Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/Custom 450 vs Custom 455

Custom 450 vs Custom 455

Property comparison of Custom 450 and Custom 455, both stainless steel.

Stainless Steel6 compared properties
PropertyCustom 450Custom 455Difference
Yield strength930.8 MPa1,276 MPa+37%
Tensile strength999.7 MPa1,379 MPa+38%
Elongation12 %10 %-17%
Elastic modulus193,053 MPa196,501 MPa+2%
Density7,750 kg/m³7,750 kg/m³0%
Reduction in area45 %40 %-11%

Difference is Custom 455 relative to Custom 450. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Custom 450
grade
Custom 450
standard
MIL-HDBK-5J
heat treatment
H1050
Custom 455
grade
Custom 455
standard
MIL-HDBK-5J
heat treatment
H1000

About 400-series stainless steels

Martensitic and ferritic stainless steels carry less nickel than the 300-series and remain magnetic. 410 and 420 are hardenable by quench and temper and are used for cutlery, shafts, and valve parts. 430 stays soft and is used for cosmetic trim and mild corrosion service. Compared to 300-series grades they trade general corrosion resistance for hardenability.