Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Cast Iron/CSN 422540 vs CSN 422555

CSN 422540 vs CSN 422555

Property comparison of CSN 422540 and CSN 422555, both cast iron.

Cast Iron11 compared properties
PropertyCSN 422540CSN 422555Difference
Yield strength180 MPa300 MPa+67%
Tensile strength400 MPa580 MPa+45%
Elongation4 %4 %0%
Elastic modulus160,000 MPa160,000 MPa0%
Shear modulus64,000 MPa64,000 MPa0%
Poisson ratio0.270.270%
Density7,160 kg/m³7,160 kg/m³0%
Thermal conductivity46 W/m·K46 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K0%
Melting point1,175 °C1,175 °C0%

Difference is CSN 422555 relative to CSN 422540. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

CSN 422540
standard
CSN
CSN 422555
standard
CSN

What else is in Engineering Database

Related comparisons

View each material