Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Cast Iron/CSN 422420 vs CSN 422540

CSN 422420 vs CSN 422540

Property comparison of CSN 422420 and CSN 422540, both cast iron.

Cast Iron10 compared properties
PropertyCSN 422420CSN 422540Difference
Yield strength200 MPa180 MPa-10%
Tensile strength200 MPa400 MPa+100%
Elastic modulus91,000 MPa160,000 MPa+76%
Shear modulus36,400 MPa64,000 MPa+76%
Poisson ratio0.250.27+8%
Density7,160 kg/m³7,160 kg/m³0%
Thermal conductivity46 W/m·K46 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K0%
Melting point1,175 °C1,175 °C0%

Difference is CSN 422540 relative to CSN 422420. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.