Property comparison of CSN 422435 and CSN 422540, both cast iron.

Cast Iron10 compared properties
PropertyCSN 422435CSN 422540Difference
Yield strength350 MPa180 MPa-49%
Tensile strength350 MPa400 MPa+14%
Elastic modulus115,000 MPa160,000 MPa+39%
Shear modulus46,000 MPa64,000 MPa+39%
Poisson ratio0.250.27+8%
Density7,160 kg/m³7,160 kg/m³0%
Thermal conductivity46 W/m·K46 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K0%
Melting point1,175 °C1,175 °C0%

Difference is CSN 422540 relative to CSN 422435. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.