Property comparison of CSN 422415 and CSN 422420, both cast iron.

Cast Iron10 compared properties
PropertyCSN 422415CSN 422420Difference
Yield strength150 MPa200 MPa+33%
Tensile strength150 MPa200 MPa+33%
Elastic modulus85,000 MPa91,000 MPa+7%
Shear modulus34,000 MPa36,400 MPa+7%
Poisson ratio0.250.250%
Density7,160 kg/m³7,160 kg/m³0%
Thermal conductivity46 W/m·K46 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K0%
Melting point1,175 °C1,175 °C0%

Difference is CSN 422420 relative to CSN 422415. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

CSN 422415
standard
CSN
CSN 422420
standard
CSN

What else is in Engineering Database

Related comparisons

View each material