CSN 422415 vs CSN 422425

Property comparison of CSN 422415 and CSN 422425, both cast iron.

Cast Iron10 compared properties
PropertyCSN 422415CSN 422425Difference
Yield strength150 MPa250 MPa+67%
Tensile strength150 MPa250 MPa+67%
Elastic modulus85,000 MPa105,000 MPa+24%
Shear modulus34,000 MPa42,000 MPa+24%
Poisson ratio0.250.250%
Density7,160 kg/m³7,160 kg/m³0%
Thermal conductivity46 W/m·K46 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K0%
Melting point1,175 °C1,175 °C0%

Difference is CSN 422425 relative to CSN 422415. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.