CSN 16527 vs CSN 17020
Property comparison of CSN 16527 and CSN 17020, both carbon steel.
| Property | CSN 16527 | CSN 17020 | Difference |
|---|---|---|---|
| Yield strength | 390 MPa | 245 MPa | -37% |
| Tensile strength | 590 MPa | 441 MPa | -25% |
| Elongation | 20 % | 21 % | +5% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 459 J/kg·K | 460 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is CSN 17020 relative to CSN 16527. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
CSN 16527
- standard
- CSN
- heat treatment
- —
CSN 17020
- standard
- CSN
- heat treatment
- normalized
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators