CSN 16430 vs CSN 16527
Property comparison of CSN 16430 and CSN 16527, both carbon steel.
| Property | CSN 16430 | CSN 16527 | Difference |
|---|---|---|---|
| Yield strength | 880 MPa | 390 MPa | -56% |
| Tensile strength | 1,080 MPa | 590 MPa | -45% |
| Elongation | 10 % | 20 % | +100% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 460 J/kg·K | 459 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is CSN 16527 relative to CSN 16430. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
CSN 16430
- standard
- CSN
- heat treatment
- heat treated
CSN 16527
- standard
- CSN
- heat treatment
- —
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators