Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/ATI 309S Austenitic Stainless Steel (Low Carbon) vs ATI 310 Austenitic Stainless Steel

ATI 309S Austenitic Stainless Steel (Low Carbon) vs ATI 310 Austenitic Stainless Steel

Property comparison of ATI 309S Austenitic Stainless Steel (Low Carbon) and ATI 310 Austenitic Stainless Steel, both stainless steel.

Stainless Steel9 compared properties
PropertyATI 309S Austenitic Stainless Steel (Low Carbon)ATI 310 Austenitic Stainless SteelDifference
Yield strength351 MPa292 MPa-17%
Tensile strength670 MPa617 MPa-8%
Elongation44.6 %45 %+1%
Elastic modulus200,000 MPa200,000 MPa0%
Shear modulus77,000 MPa77,000 MPa0%
Density8,030 kg/m³8,030 kg/m³0%
Thermal conductivity15.6 W/m·K13.8 W/m·K-12%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000016 1/K0.000016 1/K+2%

Difference is ATI 310 Austenitic Stainless Steel relative to ATI 309S Austenitic Stainless Steel (Low Carbon). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 309S Austenitic Stainless Steel (Low Carbon)
grade
309S
standard
ASTM A240; ASME SA-240
heat treatment
Annealed
ATI 310 Austenitic Stainless Steel
grade
310
standard
ASTM A167; ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.