Stainless Steel8 compared properties
PropertyATI 305 Austenitic Stainless SteelATI 309S Austenitic Stainless Steel (Low Carbon)Difference
Yield strength170 MPa351 MPa+106%
Tensile strength485 MPa670 MPa+38%
Elongation40 %44.6 %+12%
Elastic modulus200,000 MPa200,000 MPa0%
Density7,900 kg/m³8,030 kg/m³+2%
Thermal conductivity16.3 W/m·K15.6 W/m·K-4%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000017 1/K0.000016 1/K-6%

Difference is ATI 309S Austenitic Stainless Steel (Low Carbon) relative to ATI 305 Austenitic Stainless Steel. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 305 Austenitic Stainless Steel
grade
305
standard
ASTM A240
heat treatment
Annealed
ATI 309S Austenitic Stainless Steel (Low Carbon)
grade
309S
standard
ASTM A240; ASME SA-240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons

View each material