Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11) vs ATI 302 Austenitic Stainless Steel

ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11) vs ATI 302 Austenitic Stainless Steel

Property comparison of ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11) and ATI 302 Austenitic Stainless Steel, both stainless steel.

Stainless Steel8 compared properties
PropertyATI 219 Austenitic Stainless Steel (21-6-9 / XM-11)ATI 302 Austenitic Stainless SteelDifference
Yield strength465 MPa205 MPa-56%
Tensile strength780 MPa515 MPa-34%
Elongation46 %40 %-13%
Elastic modulus195,000 MPa200,000 MPa+3%
Density7,850 kg/m³7,900 kg/m³+1%
Thermal conductivity13.8 W/m·K16.3 W/m·K+18%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000017 1/K+47%

Difference is ATI 302 Austenitic Stainless Steel relative to ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11)
grade
219
standard
ASTM A240; ASTM A412; ASTM A666
heat treatment
Solution Annealed
ATI 302 Austenitic Stainless Steel
grade
302
standard
ASTM A240
heat treatment
Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.