Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/ATI 201LN Austenitic Stainless Steel (Cryogenic Grade) vs ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11)

ATI 201LN Austenitic Stainless Steel (Cryogenic Grade) vs ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11)

Property comparison of ATI 201LN Austenitic Stainless Steel (Cryogenic Grade) and ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11), both stainless steel.

Stainless Steel5 compared properties
PropertyATI 201LN Austenitic Stainless Steel (Cryogenic Grade)ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11)Difference
Yield strength320 MPa465 MPa+45%
Tensile strength685 MPa780 MPa+14%
Elongation51 %46 %-10%
Elastic modulus193,000 MPa195,000 MPa+1%
Density7,840 kg/m³7,850 kg/m³0%

Difference is ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11) relative to ATI 201LN Austenitic Stainless Steel (Cryogenic Grade). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI 201LN Austenitic Stainless Steel (Cryogenic Grade)
grade
201LN
standard
ASTM A240; ASME SA-240; ASTM A666
heat treatment
Mill Annealed
ATI 219 Austenitic Stainless Steel (21-6-9 / XM-11)
grade
219
standard
ASTM A240; ASTM A412; ASTM A666
heat treatment
Solution Annealed

About austenitic stainless steels

Austenitic stainless steels are the largest stainless family. They are non-magnetic in the annealed condition and gain corrosion resistance from chromium and nickel (and molybdenum in 316-class grades). They cannot be hardened by heat treatment and rely on cold work for higher strength. Includes the 300-series, super-austenitic grades (904L, AL-6XN), and high-nitrogen variants used in pressure vessels and chemical service.

What else is in Engineering Database

Related comparisons

View each material