Aluminum Alloy4 compared properties
PropertyAl-Li WL049 Weldalite-T6 TransverseAl-Li WL049 Weldalite-T6 45 DegreeDifference
Yield strength633.67 MPa587.33 MPa-7%
Tensile strength663.67 MPa627.67 MPa-5%
Elongation3.83 %7.43 %+94%
Density2,710 kg/m³2,710 kg/m³0%

Difference is Al-Li WL049 Weldalite-T6 45 Degree relative to Al-Li WL049 Weldalite-T6 Transverse. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Al-Li WL049 Weldalite-T6 Transverse
grade
WL049-T6
standard
NISTIR 3971
heat treatment
T6
Al-Li WL049 Weldalite-T6 45 Degree
grade
WL049-T6
standard
NISTIR 3971
heat treatment
T6