Aluminum Alloy4 compared properties
PropertyAl-Li WL049 Weldalite-T6 45 DegreeAl-Li WL049 Weldalite-T851 LongitudinalDifference
Yield strength587.33 MPa612 MPa+4%
Tensile strength627.67 MPa642 MPa+2%
Elongation7.43 %9.86 %+33%
Density2,710 kg/m³2,710 kg/m³0%

Difference is Al-Li WL049 Weldalite-T851 Longitudinal relative to Al-Li WL049 Weldalite-T6 45 Degree. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Al-Li WL049 Weldalite-T6 45 Degree
grade
WL049-T6
standard
NISTIR 3971
heat treatment
T6
Al-Li WL049 Weldalite-T851 Longitudinal
grade
WL049-T851
standard
NISTIR 3971
heat treatment
T851