Home/Compare/Stainless Steel/Al 6XN Allowable Stress vs SAE 440C Stainless Steel (Annealed bar)

Al 6XN Allowable Stress vs SAE 440C Stainless Steel (Annealed bar)

Property comparison of Al 6XN Allowable Stress and SAE 440C Stainless Steel (Annealed bar), both stainless steel.

Stainless Steel9 compared properties
PropertyAl 6XN Allowable StressSAE 440C Stainless Steel (Annealed bar)Difference
Yield strength310 MPa450 MPa+45%
Tensile strength690 MPa760 MPa+10%
Elongation35 %14 %-60%
Elastic modulus196,000 MPa193,000 MPa-2%
Density8,060 kg/m³7,850 kg/m³-3%
Brinell hardness223 HB223 HB0%
Thermal conductivity11.6 W/m·K24.7 W/m·K+113%
Coefficient of thermal expansion0.000016 1/K0.00001 1/K-35%
Melting point1,325 °C1,450 °C+9%

Difference is SAE 440C Stainless Steel (Annealed bar) relative to Al 6XN Allowable Stress. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Al 6XN Allowable Stress
grade
N08367
standard
ASTM A240/B688
heat treatment
Annealed
SAE 440C Stainless Steel (Annealed bar)
grade
440C
standard
SAE
heat treatment
Annealed bar

What else is in Engineering Database

Related comparisons

View each material