Al 6XN Allowable Stress vs Nitronic 60 Nitrogen-Strengthened
Property comparison of Al 6XN Allowable Stress and Nitronic 60 Nitrogen-Strengthened, both stainless steel.
| Property | Al 6XN Allowable Stress | Nitronic 60 Nitrogen-Strengthened | Difference |
|---|---|---|---|
| Yield strength | 310 MPa | 414 MPa | +34% |
| Tensile strength | 690 MPa | 696 MPa | +1% |
| Elongation | 35 % | 55 % | +57% |
| Elastic modulus | 196,000 MPa | 196,000 MPa | 0% |
| Density | 8,060 kg/m³ | 7,880 kg/m³ | -2% |
| Brinell hardness | 223 HB | 95 HB | -57% |
Difference is Nitronic 60 Nitrogen-Strengthened relative to Al 6XN Allowable Stress. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- N08367
- standard
- ASTM A240/B688
- heat treatment
- Annealed
- grade
- S21800
- standard
- ASTM A276
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators