5052 vs 5086

Property comparison of 5052 and 5086, both aluminum alloy.

Aluminum Alloy11 compared properties
Property50525086Difference
Yield strength193 MPa131 MPa-32%
Tensile strength228 MPa269 MPa+18%
Elongation12 %14 %+17%
Elastic modulus73,000 MPa73,000 MPa0%
Shear modulus26,000 MPa26,000 MPa0%
Poisson ratio0.330.330%
Density2,700 kg/m³2,700 kg/m³0%
Thermal conductivity117 W/m·K117 W/m·K0%
Specific heat880 J/kg·K900 J/kg·K+2%
Coefficient of thermal expansion0.000024 1/K0.000024 1/K0%
Melting point568 °C568 °C0%

Difference is 5086 relative to 5052. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

5052
standard
ANSI
heat treatment
Wrought
5086
standard
ANSI
heat treatment
Wrought

About 5xxx aluminum alloys

5xxx aluminum alloys are alloyed with magnesium. They are not heat-treatable and gain strength through cold work. They have the best corrosion resistance of the wrought aluminums in marine environments. 5052 covers general sheet work; 5083 and 5086 are common in shipbuilding and pressure vessels.