Property20262219Difference
Yield strength372.33 MPa409 MPa+10%
Tensile strength503.34 MPa496.75 MPa-1%
Elongation10 %13.35 %+34%
Elastic modulus73,777 MPa81,200 MPa+10%
Shear modulus27,580 MPa30,600 MPa+11%
Poisson ratio0.330.325-2%
Density2,768 kg/m³2,820 kg/m³+2%

Difference is 2219 relative to 2026. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

2026
grade
2026
standard
MIL-HDBK-5J
heat treatment
Wrought
2219
grade
2219-T87
standard
NISTIR 3971
heat treatment
T87

About 2xxx aluminum alloys

2xxx aluminum alloys are alloyed with copper. They reach the highest strengths in the wrought aluminum family but corrode faster than 5xxx or 6xxx and are difficult to weld. 2024 is the aerospace standard for skin and structure; 2014 is used for forgings.