brinell hardnesscategorycte per Kdensity kg m3elastic modulus MPaelongation percentgradeheat treatmentmaterial idmelting point Cnamepoisson ratioreduction percentshear modulus MPaspecific heat J kgKstandardtensile strength MPathermal conductivity W mKyield strength MPa
419stainless_steel0.000017,850193,00017431Oil quenched from 980°C (1800 °F); tempered at 40 °C (104 °F)SAE_431_Stainless_Steel_Oil_quenched_from_980°C_1800_°F;_tempered_at_40_°C_104_°F1,450SAE 431 Stainless Steel (Oil quenched from 980°C (1800 °F); tempered at 40 °C (104 °F)0.35974,230.8460SAE1,43524.71,140